Catalysts & Adsorbents

Description

shutterstock_220655650-catalyst

Catalysts are generally used to lower the energy input necessary for a chemical reaction to occur and to increase the corresponding reaction rate. On the industrial scale, it allows running reactions at lower temperatures.
Catalytic reaction schemes often go through a first step of adsorption of at least one of the reactants, and can thus be studied as simple adsorbents. Adsorbents such as zeolites, active carbons, MOF’S are also investigated for their properties of gas storage (hydrogen, C02). Thermogravimetric analysis (TGA) and volumetry are techniques allowing the quantification of the adsorbate, and calorimetry provides key data for the determination of the strength and nature of the interactions.

–    Solid-gas reaction (gas sorption)
–    Characterization of acidity and basicity
–    Homogeneous  and heterogeneous catalysis
–    Regeneration of a catalyst
–    Adsorption / Absorption / Desorption

Some International References
Université de Liège – Belgium
Faculté Polytechnique de Mons – Belgium

Associated products

TGA, from ambient to 1150°C or 1600°C

LABSYS evo TGA

LABSYS evo is a user friendly, robust and highly powerful thermal analysis platform. HIGHLIGHTS include: • A comprehensive line of thermal analyzers with two temperature ranges chosen and optimized for distinct families of application: – RT – 1 150 °C, a cost effective solution mostly (but not only)...

Read more »

TGA, and Simultaneous TGA-DTA, TGA-DSC from ambient to 1150°C or 1600°C

LABSYS evo STA

LABSYS evo is a user friendly, robust and highly powerful thermal analysis platform. HIGHLIGHTS include: • A comprehensive line of thermal analyzers with two temperature ranges chosen and optimized for distinct families of application: – RT – 1 150 °C, a cost effective solution...

Read more »

Customized solutions

You’re being told it won’t work? Let’s find a solution together! High end research and development require more and more specialized analytical equipment. Today, one cannot trust anymore experimental data acquired under conditions that are far away from the true conditions of use of materials. Moreover, researchers want to acquire more and more information from...

Read more »

High-performance simultaneous TGA & DTA / DSC (ambient / 2400°C) with Evolved Gas Analysis

SETSYS Evolution TGA/STA-EGA

  The HIGHLIGHTS SETSYS Evolution is the standard for high performance TGA, TG-DSC and TG-DTA application.  It is based on a complete modular thermal analysis platform for – TGA, DTA and DSC – Simultaneous TGA/DTA and TGA/DSC – The key to...

Read more »

TGA-EGA and Simultaneous STA-EGA, from ambient to 1150°C or 1600°C

LABSYS evo TGA/STA-EGA

THE HIGHLIGHTS Simplicity of use: thanks to both an ergonomic design and the dedicated market leading Calisto software, LABSYS evo is user friendly and intuitive to operate – LABSYS evo offers a “Plug & play” gas analyzer coupling device,enabling simultaneous MS, FTIR or GC/MS connections....

Read more »

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: TG-DSC-EGA

SENSYS evo TG-DSC-EGA

  The HIGHLIGHTS Thermogravimetry Excellent TG signal baseline: the symmetry of the microbalance, with its sample and reference suspended vertically from the beam guarantee reproducible positioning of the sample over time and excellent stability of the TG signal baseline. Automatic compensation of...

Read more »

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG - DSC - coupling to gas analyzer

SENSYS evo DSC

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG – DSC – coupling to gas analyzer The HIGHLIGHTS Incomparable precision: the unique 3D sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you an...

Read more »

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TGA-DSC-coupling to gas analyzer

SENSYS evo TGA-DSC

The HIGHLIGHTS Differential Scanning Calorimeter – Incomparable precision: the unique 3D DSC sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you...

Read more »

High Performance Symmetrical TGA System (ambient / 1750°C)

TAG

– Outstanding isothermal balance performance for long term corrosion/oxidation studies – No buoyancy effect with dual furnace design for high precision DTA/DSC – Unique sample geometry for near 100% surface area studies – Mass Spectrometry Coupling – Calisto software The TAG system is the world’s most precise...

Read more »

A fully automated Sieverts instrument for measuring gas (CO2, CH4, C2H6, N2, H2) sorption properties of materials

PCTPro

The PCTPro is based on the Sievert’s method. A sample at known pressure and volume is connected to a reservoir of known volume and pressure through an isolation valve. Opening the isolation valve allows new equilibrium to be...

Read more »