Calorimetry

Calorimetry : BT 2.15

BT 2.15 (calorimetry)

Low Temperature Calorimetry (from -196°C to 200°C) The BT2.15 calorimeter permits studying all freezing and crystallization phenomena at very low temperatures for different products (oils, polymers, hydrates, materials for construction and superconductors).  A sister product to the world famous C80, the BT 2.15 gives the benefits of large volumes coupled with the unique ability to […]

Calorimetry : LABSYS evo DTA/DSC

LABSYS evo DTA/DSC (thermal analysis)

DTA, DSC from ambient to 1150°C or 1600°C LABSYS evo is a user friendly, robust and highly powerful thermal analysis platform. HIGHLIGHTS include: • A comprehensive line of thermal analyzers with two temperature ranges chosen and optimized for distinct families of application: – RT – 1 150 °C, a cost effective solution mostly (but not […]

Calorimetry : microSC-4c

microSC-4c (microcalorimetry)

Microcalorimetry (- 20°C to 170°C) Highlights include: – Wide temperature range covering -20 to 170°C – 2 measuring cells, featuring zero cross talk, and easily removable and reusable cells – High precision isothermal and scanning options are available to enable the study of both transitions and long term isothermal behaviour, such as stability and long […]

Calorimetry : C80

C80 (calorimetry)

Reaction, isothermal and scanning calorimeter (ambient to 300°C) Incomparable precision of measurement: the 3D Calvet sensor totally surrounds the sample, and all heat evolved is measured. Now matter how small or large the thermal transformation the system provides a complete picture of the event. Absolute calibration: with a three-dimensional transducer the sensitivity of the C80 […]

Calorimetry : AlexSys

AlexSys (high temperature calorimetry)

High Temperature 3D Calvet Calorimeter (up to 800 / 1000°C) Sensitivity, stability, flexibility and precision: The AlexSys calorimeter features a 3D Calvet sensor, providing high sensitivity and exceptional precision. The calorimeter block and furnace design ensures a high signal-to-noise ratio,temperature and signal stability, and low detection limit permitting low energy and slow reactions to be […]

Calorimetry : MS80

MS80 (calorimetry)

Very High Sensitivity Isothermal Calorimeter (ambient to 200°C) The MS80 calorimeter has the greatest sensitivity in the Calvet 3D calorimeter range. It is mostly used in isothermal mode, between ambient temperature and + 200°C, and is intended for measurements of very low thermal effects: self-discharge of batteries, self-decomposition of powders, heat generation of plants and […]

Calorimetry : C600

C600 (calorimetry)

Isothermal and temperature scanning calorimeter (ambient to 600°C) The C600 high temperature Calvet calorimeter is based on the 3D Calvet sensor technology. An array of thermocouples totally surrounds the sample, and all the heat evolved is measured. No matter how small or large the thermal transformation, the system provides a complete picture of the event. […]

Calorimetry : MHTC 96

MHTC 96 (high temperature calorimetry)

Large-volume, High-Temperature DSC and (drop) calorimeter (ambient to 1600°C) The requirements of different experiments are sometimes contradictory, e.g. low sample mass is needed for good transition detection, high sample mass for accurate determination of heat capacity; analysis may need constant or variable temperature; use of the crucible may be open or closed. Two types of […]

Calorimetry : microDSC7 evo

microDSC7 evo (microcalorimetry)

High-sensitivity DSC and microcalorimetry (-45 to 120°C) The HIGHLIGHTS • Wide operating temperature range (from -45 °C to 120 °C): cooling of the calorimeter does not require an external source. • Use in isothermal or temperature programming (DSC) mode. • Possibility to study samples in all forms: liquids, gel, powder, solid. • Variety of closed […]