SENSYS evo TG-DSC (simultaneous thermal analysis)

the highlights

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TGA-DSC-coupling to gas analyzer

Differential Scanning Calorimeter

– Incomparable precision: the unique 3D DSC sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you an unequalled accuracy of measurement.

– Parameter Independent Calibration: because of the 3D transducer the calibration of SENSYS evo is independent of:
– mass and form (powder, fibre, liquid, etc.) of the sample,
– contact between the sample and the transducer,
– crucible type,
– sweeping gas (inert, oxidizing, reducing, wet, pressure) and flow rate.


– Excellent TG signal baseline: the symmetry of the microbalance, with its sample and reference suspended vertically from the beam guarantee reproducible positioning of the sample over time and excellent stability of the TG signal baseline.

– Automatic compensation of Buoyancy: the sample and the reference are heated inside the same calorimetric block (symmetrical furnace), which means that the buoyancy effect is automatically compensated.

Ease of operation: dedicated market leading CALISTO software that is not only intuitive but powerful enough to perform every typical experiments and data treatment.


2D plate-shaped or cylindrical 3D Calvet sensor?

Temperature range Ambient to 830 °C
With cooling accessories -120 °C to 200 °C (Liquid Nitrogen Accessory)
Temperature accuracy +/-0.1 °C
Temperature precision +/-0.02 °C
Programmable temperature scanning rate(heating and cooling) 0.01 to 30 °C min-1
Cooling time 17 min (from 50 °C to -100 °C)with Liquid Nitrogen Accessory
Enthalpy accuracy +/-1 %
Calorimetric Precision +/-0.1 %
RMS Noise 0.2 μW
Sensitivity (Joule effect at 30°C) 6.7 μV/mW
Resolution 0.35 μW / 0.035 μW
Dynamic range Resolution +/-2500 mW
Gases 3 carrier gases ((MFC from 4 to 200 ml/min) + 11 auxiliary or reactive gas (MFC from 0.3 to 16 ml/min)
Crucibles 120 μl, 160 μl, 320 μl – aluminium, incoloy, gold plated incoloy, graphite,alumina, platinum, etc.
Pressure (non controlled) High Pressure Crucible (up to 500 bars / 7250 psi at 600 °C)
Pressure (measured & controlled) High Pressure Crucible (up to 400 bars / 5800 psi at 600 °C)
TG $$
Maximum balance capacity 3 g
Weight range +/-200 mg
Weighing precision +/-0.01 %
TG Resolution 0.02 μg, 0.002 μg
Baseline dynamic drift < 10 μg
Isothermal temperature accuracy +/-0.1 °C
Linear heating rate 30 °C/min
Vacuum < 10-1 mbar
Evolved gas MS, FTIR, GC couplings
Weight 55 kg (121 lbs)
Dimensions (Height / Width / Depth) 60 closed, 80 opened / 53 / 58 cm (23,6 closed, 31.4 opened / 20.9 / 22.8 in)
Power requirements 230 V – 50/60 Hz

CRUCIBLES Crucibles of 150 μl capacity are available in aluminium, alumina, platinum or silica to suit the chemical nature of the sample. A silica tube can be added to protect the transducer and the analysis chambers during test involving sweeping with corrosive gas. Evolved Gas Analysis The SENSYS evo design features both a small furnace volume and also an easily accessible exhaust to allow for direct connection to further analysis devices such as MS, FTIR, GC etc. without excessive sample dilution or long transfer lines. Setaram offers a range of transfer lines and software solution for system comprehensive integration. To date SENSYS has also been successfully coupled with: – FTIR/MS and GC, – Gas Sorption devices, – An X-ray absorption spectroscopy apparatus. Measurements under controlled humidity Humidity is known to have a significant influence on the stability of many materials. In order to evaluate this specific influence, SETARAM has developed WETSYS a controlled humidity generator. It can: – deliver a very precise level of relative humidity (RH) from 5 to 95 % depending on the temperature and measure the humidity around the sample. – be connected to SETARAM instruments, and in particular to the SENSYS evo TGA-DSC as well as other analysis instrument(RX, GC, etc.) for studies of sorption, hydration, stability, etc.


Applications With its high precision and wide temperature range (-120 to 830 °C) the SENSYS evo TGA-DSC has a wide range of applications, especially in the fields of thermodynamics (Specific Heat Capacity Cp precision within +/-1 %), pharmaceuticals (phase diagram, polymorphism, purity, thermal stability), safety of chemical process (transition, decomposition under high pressure), energy (catalysis, hydrogen storage, hydrogen adsorption),polymers (glass transition, measurement under pressure), etc. View the application notes in your field, available for download, by visiting Application Library area We have also included a powerful search engine that will enable you to find the most applicable data.


Application notes

This an extract of our documentation, please register to have access to all documentation.

associated products
Thermogravimetry (TGA) : SENSYS evo TGA-DSC par SETARAM