Metal-based inorganic nanoparticles are one of the most studied materials due to their innumerable applications. Moreover, the compound functionalization with organic ligands results essential for some uses, e.g. in drug delivery technology. Even if several techniques are common available to establish size, structure and morphology of the particles, the identification of the quantity and the way in which the
ligands are attached on their surface is not trivial.