Fuel Cell & Hydrogen

Description

voiture-hybride-ref-2351

The storage of hydrogen and the development of fuel cells are one of the main issues for the development of renewable energies in the next few years. Different groups of materials have the potentiality to store and release hydrogen:
–    carbon : nanotubes and graphite nanofibers
–    other high surface area materials :
– H2O-reactive chemical hydrides: zeolites, gas hydrates, metal oxide frameworks (MOFs)
– thermal chemical hydrides
– rechargeable hydrides borohydrides, alanates, amides.

The R&D issues that can be followed by the calorimetric techniques are to find lower desorption temperatures, higher desorption kinetics, optimization of the recharge time and pressure, heat management, cyclic life, optimization of the storage capacity.

Some International References
LCMTR Thiais – France
TU Bergakademie Freiberg – Germany

 

Associated products

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG - DSC - coupling to gas analyzer

SENSYS evo DSC

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG – DSC – coupling to gas analyzer The HIGHLIGHTS Incomparable precision: the unique 3D sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you an...

Read more »

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TGA-DSC-coupling to gas analyzer

SENSYS evo TGA-DSC

The HIGHLIGHTS Differential Scanning Calorimeter – Incomparable precision: the unique 3D DSC sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you...

Read more »

A fully automated Sieverts instrument for measuring gas (CO2, CH4, C2H6, N2, H2) sorption properties of materials

PCTPro

The PCTPro is based on the Sievert’s method. A sample at known pressure and volume is connected to a reservoir of known volume and pressure through an isolation valve. Opening the isolation valve allows new equilibrium to be...

Read more »

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG-DSC-coupling to gas analyzer

SENSYS evo TG-DSC

The HIGHLIGHTS Differential Scanning Calorimeter – Incomparable precision: the unique 3D DSC sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you...

Read more »

High-performance modular DTA & DSC thermal analyzers (ambient / 2400°C)

SETSYS Evolution DTA/DSC

The HIGHLIGHTS SETSYS Evolution is the standard for high performance TGA, TG-DSC and TG-DTA application.  It is based on a complete modular thermal analysis platform for – TGA, DTA and DSC – Simultaneous TGA/DTA and TGA/DSC – Dilatometry / TMA The key to the SETSYS...

Read more »

High-performance modular Thermogravimetric Analysis (TGA) (ambient / 2400°C)

SETSYS Evolution TGA

The HIGHLIGHTS SETSYS Evolution is the standard for high performance thermogravimetric analysis (TGA) , TG-DSC and TG-DTA application.  It is based on a complete modular thermal analysis platform for – TGA, DTA and DSC – Simultaneous TGA/DTA and TGA/DSC – Dilatometry / TMA The key to the SETSYS...

Read more »

High-performance modular simultaneous TGA & DTA / DSC thermal analyzer (ambient / 2400°C)

SETSYS Evolution TGA-DTA/DSC

SETSYS Evolution is the standard for high performance TGA, TG-DSC and TG-DTA application.  It is based on a complete modular thermal analysis platform for – TGA, DTA and DSC – Simultaneous TGA/DTA and TGA/DSC – Dilatometry / TMA The key to the...

Read more »

High-performance Modular Thermo Mechanical Analysis (TMA) (ambient / 2400°C)

SETSYS Evolution TMA

The HIGHLIGHTS SETSYS Evolution is the standard for high performance TG, TG-DSC and TG-DTA application.  It is based on a complete modular thermal analysis platform for – TGA, DTA and DSC – Simultaneous TGA/DTA and TGA/DSC – Dilatometry/ Thermo Mechanical Analysis (TMA) The key to the SETSYS TMA is...

Read more »

Mastering High Pressure DSC & Microcalorimetry up to 1000 bars - 14,500 psi

HP Micro DSC

Mastering High Pressure DSC & Microcalorimetry up to 1000 bars – 14,500 psi Originally designed under a IFP (Institut Français du Petrole) license to study the gas hydrates formation and dissociation, the high pressure version of the μDSC7 evo offers unique capabilities on the market: on a wide temperature range, from the subambient temperature of...

Read more »

Reaction, isothermal and scanning calorimeter (ambient to 300°C)

C80

Incomparable precision of measurement: the 3D Calvet sensor totally surrounds the sample, and all heat evolved is measured. Now matter how small or large the thermal transformation the system provides a complete picture of the event. Absolute calibration: with a three-dimensional transducer the sensitivity of the C80...

Read more »

Documentation

Brochures
Application notes
Articles See articles