Glasses

Description

glass-calorymetry

Although glass is a very common material, its increasing technicality for special applications, and issues linked with its worldwide scale manufacturing requires state of the art analytic tools.

Apart from the famous glass transition temperature, which corresponds to the softening of the glass, DSC can become a key technique to study melting, crystallization and other phase transitions.

High temperature calorimetry becomes also very useful when process data such as heat capacity are to be measured.
–  Glass transition
–  Phase transition
Design of baking furnace

Some References
Saint Gobain – France
CEMHTI Orléans – France

Associated products

TX

TX Touch Experience Platform – The fastest, easiest way to measure thermal conductivity and effusivity The C-Therm TCi employs the patented Modified Transient Plane Source (MTPS) technique. The one-sided, interfacial heat reflectance sensor applies a momentary constant heat source to the sample. Thermal conductivity and effusivity are measured directly, providing a detailed overview of the...

Read more »

High Pressure TGA up to 1200°C and 150 bar

THEMYS HP TGA

The THEMYS is the NEW benchmark for modular thermogravimetric analysis. The THEMYS is available in various platforms: Standard Thermogravimetric Analysis (TGA), high pressure TGA, Simultaneous Thermal Analysis (STA) TG/DSC, Differential Thermal Analysis / Differential Scanning Calorimetry (DTA/DSC), and Evolved Gas Analysis (EGA). The design of the...

Read more »

Simultaneous Thermal Analysis Platform (STA) with Evolved Gas Analysis (EGA) from ambient to 1600°C

THEMYS TGA/STA-EGA (Evolved Gas Analysis)

The THEMYS is the NEW benchmark for modular thermogravimetric analysis. The THEMYS is available in various platforms: Standard Thermogravimetric Analysis (TGA), high pressure TGA, Simultaneous Thermal Analysis (STA) TG/DSC, Differential Thermal Analysis / Differential Scanning Calorimetry (DTA/DSC), and Evolved Gas Analysis...

Read more »

Simultaneous Thermal Analyzer (TGA/DSC – DTA) up to 1750°C

THEMYS STA (Simultaneous Thermal Analysis)

The THEMYS is the NEW benchmark for modular thermogravimetric analysis. The THEMYS is available in various platforms: Standard Thermogravimetric Analysis (TGA), high pressure TGA, Simultaneous Thermal Analysis (STA) TG/DSC, Differential Thermal Analysis / Differential Scanning Calorimetry (DTA/DSC), and Evolved Gas Analysis (EGA). The design of the...

Read more »

TGA, from ambient to 1150°C or 1600°C

LABSYS evo TGA

LABSYS evo is a user friendly, robust and highly powerful thermal analysis platform. HIGHLIGHTS include: • A comprehensive line of thermal analyzers with two temperature ranges chosen and optimized for distinct families of application: – RT – 1 150 °C, a cost effective solution mostly (but not only)...

Read more »

DTA, DSC from ambient to 1150°C or 1600°C

LABSYS evo DTA/DSC

LABSYS evo is a user friendly, robust and highly powerful thermal analysis platform. HIGHLIGHTS include: • A comprehensive line of thermal analyzers with two temperature ranges chosen and optimized for distinct families of application: – RT – 1 150 °C, a cost effective solution mostly (but not...

Read more »

TGA, and Simultaneous TGA-DTA, TGA-DSC from ambient to 1150°C or 1600°C

LABSYS evo STA

LABSYS evo is a user friendly, robust and highly powerful thermal analysis platform. HIGHLIGHTS include: • A comprehensive line of thermal analyzers with two temperature ranges chosen and optimized for distinct families of application: – RT – 1 150 °C, a cost effective solution...

Read more »

Customized solutions

You’re being told it won’t work? Let’s find a solution together! High end research and development require more and more specialized analytical equipment. Today, one cannot trust anymore experimental data acquired under conditions that are far away from the true conditions of use of materials. Moreover, researchers want to acquire more and more information from...

Read more »

Horizontal dilatometer (room temperature / 1200°C)

C-Therm Dilatometer

  The HIGHLIGHTS: C-Therm dilatometers offer high resolution and stability across a broad measurement range. With unparalleled ease-of-use, high adaptability, and modular design, C-Therm dilatometers offer researchers a robust cost-effective solution to their characterization needs.   See also: SETSYS Evolution TMA, TCi

Large volume & high temperature TGA/STA-EGA (ambient to 2000°C)

96 Line TGA/STA-EGA

This is an extremely high performance weighing module used with the TGA 96. This balance can weigh samples up to 100 g and is well suited to measuring both micro-quantities of samples (a few milligrams) as well as large, dense samples while maintaining measurement resolution to...