Microcalorimetry (- 20°C to 170°C)

Highlights include:

– Wide temperature range covering -20 to 170°C

– 2 measuring cells, featuring zero cross talk, and easily removable and reusable cells

– High precision isothermal and scanning options are available to enable the study of both transitions and long term isothermal behaviour, such as stability and long term reaction

– 2-cell version is also available upon request (microSC-2c).

 

2D plate-shaped or cylindrical 3D Calvet sensor?

specifications
Temperature range – 20°C to 170°C
Programmable temperature scanning rate (heating and cooling) From 0.001 to 1.2 °C.min-1
RMS noise 0.2 µW typical
Measurement Cells 2 X 1ml – Made of Hastelloy C – removable no signal cross contamination between cells (up to 10mW)
2-cell version is also available upon request (microSC-2c)
Weight 37.4 kg (82.5 lbs)
Dimensions 40 / 53 / 58 cm (15.7 / 20.9 / 22.8 in)
Power requirement 230v – 50/60 Hz
applications

With its temperature range (-20 to 170°C) the µSC can meet a wide range of applications, especially when dealing with : Pharmaceuticals: – crystallization of amorphous phase of excipients, – purity, polymorphism of API ( the sensitivity improves the lower % of detectable amorphous phase)  – API-Excipient compatibility Energetic Materials: Thermal activity of propellants Food: – degree of gelatinization of cereals, starch,  polysaccharides – thermal denaturation of proteins – oxygen induction times of lipids – Maillard reaction on polysaccharides, proteins interactions – Phase transition

cells
calorimetrythumb_cellule_104-3
calorimetrythumb_cellule_105-3
documentation


Brochures

This an extract of our documentation, please register to have access to all documentation.



Differential Scanning Calorimetry (DSC)/ Differential Thermal Analysis (DTA) : microSC-4c par SETARAM